YLW-100 Slow Strain Rate Tension (SSRT) Stress Corrosion Testing Machine Product Information

YLW-20 Slow Strain Rate Tension (SSRT) Stress Corrosion Material Testing Machine Product Information
June 22, 2017
DTS-1200 Measuring and Controlling System for Pressure Testing Machine Product Information
June 22, 2017

YLW-100 Slow Strain Rate Tension (SSRT) Stress Corrosion Testing Machine Product Information


  • Version
  • 1872 Download
  • 56.77 KB File Size
  • June 22, 2017 Create Date

YLW-100 slow strain rate tension (SSRT) stress corrosion testing machine is mainly used to test and study the mechanical properties test of static persistent tensile, creep and stress corrosion of metallic materials.
It can be used in the characteristic tests of metal stress corrosion damage in a variety of media environments as NaOH, NO3, H2S, CL solution, methanol, N2O4, NH3, wet air and water.